Property | Value |
---|---|
Dimensions | Round-Bar length: 10-80 mm |
Mecánica
Property | Value |
---|---|
Resistencia a la tracción | 500.0 - 750.0 MPa Show Supplier Material materials with Resistencia a la tracción of 500.0 - 750.0 MPa |
Chemical properties
Property | Value | Comment |
---|---|---|
Azufre | 0.03 % Show Supplier Material materials with Azufre of 0.03 % | max. |
Carbono | 0.4 - 0.5 % Show Supplier Material materials with Carbono of 0.4 - 0.5 % | |
Cromo | 17.0 - 19.0 % Show Supplier Material materials with Cromo of 17.0 - 19.0 % | |
Fósforo | 0.045 % Show Supplier Material materials with Fósforo of 0.045 % | max. |
Manganeso | 0.8 - 1.5 % Show Supplier Material materials with Manganeso of 0.8 - 1.5 % | |
Níquel | 8.0 - 10.0 % Show Supplier Material materials with Níquel of 8.0 - 10.0 % | |
Silicona | 2.0 - 3.0 % Show Supplier Material materials with Silicona of 2.0 - 3.0 % | |
Wolframio | 0.8 - 1.2 % Show Supplier Material materials with Wolframio of 0.8 - 1.2 % |
Technological properties
Property | ||
---|---|---|
Application areas | Plant construction, Apparatus engineering, Power Generation, Power plants | |
Processing history | Solution Annealed |