Medidas
Property | Value |
---|---|
Dimensions | Round-Bar length: 6-270 mm |
Mecánica
Property | Value |
---|---|
Resistencia a la tracción | 550.0 - 750.0 MPa Show Supplier Material materials with Resistencia a la tracción of 550.0 - 750.0 MPa |
Chemical properties
Property | Value | Comment |
---|---|---|
Aluminio | 0.04 % Show Supplier Material materials with Aluminio of 0.04 % | max. |
Azufre | 0.015 % Show Supplier Material materials with Azufre of 0.015 % | max. |
Carbono | 0.08 - 0.12 % Show Supplier Material materials with Carbono of 0.08 - 0.12 % | |
Cromo | 8.0 - 9.5 % Show Supplier Material materials with Cromo of 8.0 - 9.5 % | |
Fósforo | 0.025 % Show Supplier Material materials with Fósforo of 0.025 % | max. |
Manganeso | 0.3 - 0.6 % Show Supplier Material materials with Manganeso of 0.3 - 0.6 % | |
Molibdeno | 0.85 - 1.05 % Show Supplier Material materials with Molibdeno of 0.85 - 1.05 % | |
Nitrógeno | 0.03 - 0.07 % Show Supplier Material materials with Nitrógeno of 0.03 - 0.07 % | |
Níquel | 0.4 % Show Supplier Material materials with Níquel of 0.4 % | max. |
Silicona | 0.5 % Show Supplier Material materials with Silicona of 0.5 % | max. |
Vanadio | 0.18 - 0.25 % Show Supplier Material materials with Vanadio of 0.18 - 0.25 % |
Technological properties
Property | ||
---|---|---|
Application areas | Mechanical engineering, Apparatus engineering, Ship building, Pressure vessels and steam boiler construction, Chemical industry | |
Processing history | Solution Annealed |