Medidas
Property | Value |
---|---|
Dimensions | Round-Bar length: 6-500 mm |
Mecánica
Property | Value | Comment |
---|---|---|
Dureza Brinell | 270.0 - 311.0 [-] Show Supplier Material materials with Dureza Brinell of 270.0 - 311.0 [-] | |
Elongación | 12 % Show Supplier Material materials with Elongación of 12 % | min. |
Límite elástico | 750.0 MPa Show Supplier Material materials with Límite elástico of 750.0 MPa | min., RP02 |
Resistencia a la tracción | 900.0 - 1050.0 MPa Show Supplier Material materials with Resistencia a la tracción of 900.0 - 1050.0 MPa |
Chemical properties
Property | Value | Comment |
---|---|---|
Azufre | 0.015 % Show Supplier Material materials with Azufre of 0.015 % | max. |
Boro | 0.0015 - 0.005 % Show Supplier Material materials with Boro of 0.0015 - 0.005 % | |
Carbono | 0.04 % Show Supplier Material materials with Carbono of 0.04 % | max. |
Cromo | 10.0 - 18.0 % Show Supplier Material materials with Cromo of 10.0 - 18.0 % | |
Fósforo | 0.035 % Show Supplier Material materials with Fósforo of 0.035 % | max. |
Manganeso | 2.0 % Show Supplier Material materials with Manganeso of 2.0 % | max. |
Molibdeno | 2.0 - 3.0 % Show Supplier Material materials with Molibdeno of 2.0 - 3.0 % | |
Nitrógeno | 0.1 - 0.18 % Show Supplier Material materials with Nitrógeno of 0.1 - 0.18 % | |
Níquel | 12.0 - 14.0 % Show Supplier Material materials with Níquel of 12.0 - 14.0 % | |
Silicona | 0.75 % Show Supplier Material materials with Silicona of 0.75 % | max. |
Technological properties
Property | ||
---|---|---|
Application areas | Connecting parts, High temperature resistant components, Nuts, Screws | |
Processing history | Quenched and Tempered |