Medidas
Property | Value |
---|---|
Dimensions | Round-Bar length: 5-525 mm - Hexagonal Bar: 13- 60 mm |
Mecánica
Property | Value | Comment |
---|---|---|
Dureza Brinell | 245.0 - 285.0 [-] Show Supplier Material materials with Dureza Brinell of 245.0 - 285.0 [-] | |
Elongación | 14 % Show Supplier Material materials with Elongación of 14 % | min. |
Límite elástico | 600.0 MPa Show Supplier Material materials with Límite elástico of 600.0 MPa | min., RP02 |
Resistencia a la tracción | 800.0 - 950.0 MPa Show Supplier Material materials with Resistencia a la tracción of 800.0 - 950.0 MPa |
Chemical properties
Property | Value | Comment |
---|---|---|
Azufre | 0.015 % Show Supplier Material materials with Azufre of 0.015 % | max. |
Carbono | 0.17 - 0.23 % Show Supplier Material materials with Carbono of 0.17 - 0.23 % | |
Cromo | 10.0 - 12.5 % Show Supplier Material materials with Cromo of 10.0 - 12.5 % | |
Fósforo | 0.025 % Show Supplier Material materials with Fósforo of 0.025 % | max. |
Manganeso | 0.3 - 1.0 % Show Supplier Material materials with Manganeso of 0.3 - 1.0 % | |
Molibdeno | 0.8 - 1.2 % Show Supplier Material materials with Molibdeno of 0.8 - 1.2 % | |
Níquel | 0.3 - 0.8 % Show Supplier Material materials with Níquel of 0.3 - 0.8 % | |
Silicona | 0.4 % Show Supplier Material materials with Silicona of 0.4 % | max. |
Vanadio | 0.2 - 0.35 % Show Supplier Material materials with Vanadio of 0.2 - 0.35 % |
Technological properties
Property | ||
---|---|---|
Application areas | Power plant engineering, Mechanical Engineering, Power Generation, Components for reactor technology, chemical industry and turbines, steam boiler and pipeline construction | |
Processing history | Quenched and Tempered |