Medidas
Property | Value |
---|---|
Dimensions | Round-Bar length: 9-80 mm |
Chemical properties
Property | Value | Comment |
---|---|---|
Azufre | 0.015 % Show Supplier Material materials with Azufre of 0.015 % | max. |
Carbono | 0.18 - 0.24 % Show Supplier Material materials with Carbono of 0.18 - 0.24 % | |
Cromo | 11.0 - 12.5 % Show Supplier Material materials with Cromo of 11.0 - 12.5 % | |
Fósforo | 0.025 % Show Supplier Material materials with Fósforo of 0.025 % | max. |
Manganeso | 0.4 - 0.9 % Show Supplier Material materials with Manganeso of 0.4 - 0.9 % | |
Molibdeno | 0.8 - 1.2 % Show Supplier Material materials with Molibdeno of 0.8 - 1.2 % | |
Níquel | 0.3 - 0.8 % Show Supplier Material materials with Níquel of 0.3 - 0.8 % | |
Silicona | 0.5 % Show Supplier Material materials with Silicona of 0.5 % | max. |
Vanadio | 0.25 - 0.35 % Show Supplier Material materials with Vanadio of 0.25 - 0.35 % |
Technological properties
Property | ||
---|---|---|
Application areas | Power plant engineering, Mechanical Engineering, Power Generation, Aerospace, Parts for gas turbines and engines like runners, discs, shafts, screws, extension rings, fittings, housings | |
Processing history | Hardened |