Medidas
Property | Value |
---|---|
Dimensions | Round-Bar length: 6.5-310 mm - Hexagonal Bar: 13- 60 mm |
Mecánica
Property | Value | Comment |
---|---|---|
Dureza Brinell | 248.0 - 341.0 [-] Show Supplier Material materials with Dureza Brinell of 248.0 - 341.0 [-] | |
Elongación | 16 % Show Supplier Material materials with Elongación of 16 % | min. |
Límite elástico | 600.0 MPa Show Supplier Material materials with Límite elástico of 600.0 MPa | min., RP02 |
Resistencia a la tracción | 900.0 - 1150.0 MPa Show Supplier Material materials with Resistencia a la tracción of 900.0 - 1150.0 MPa |
Chemical properties
Property | Value | Comment |
---|---|---|
Azufre | 0.015 % Show Supplier Material materials with Azufre of 0.015 % | max. |
Carbono | 0.04 - 0.1 % Show Supplier Material materials with Carbono of 0.04 - 0.1 % | |
Cromo | 15.0 - 17.0 % Show Supplier Material materials with Cromo of 15.0 - 17.0 % | |
Fósforo | 0.035 % Show Supplier Material materials with Fósforo of 0.035 % | max. |
Manganeso | 1.5 % Show Supplier Material materials with Manganeso of 1.5 % | max. |
Níquel | 24.0 - 27.0 % Show Supplier Material materials with Níquel of 24.0 - 27.0 % | |
Silicona | 0.3 - 0.6 % Show Supplier Material materials with Silicona of 0.3 - 0.6 % | |
Titanio | 0.0001 % Show Supplier Material materials with Titanio of 0.0001 % | max. |
Technological properties
Property | ||
---|---|---|
Application areas | Power plant engineering, Mechanical Engineering, Power Generation, Parts for gas turbines and engines like runners, discs, shafts, screws, extension rings, fittings, housings | |
Processing history | Hardened |