Medidas
Property | Value |
---|---|
Dimensions | Round-Bar length: 14.52-115 mm - Hexagonal Bar: 24- 55 mm |
Mecánica
Property | Value | Comment |
---|---|---|
Dureza Brinell | 200.0 - 260.0 [-] Show Supplier Material materials with Dureza Brinell of 200.0 - 260.0 [-] | |
Elongación | 17 % Show Supplier Material materials with Elongación of 17 % | min. |
Límite elástico | 500.0 MPa Show Supplier Material materials with Límite elástico of 500.0 MPa | min., RP02 |
Resistencia a la tracción | 650.0 - 850.0 MPa Show Supplier Material materials with Resistencia a la tracción of 650.0 - 850.0 MPa |
Chemical properties
Property | Value | Comment |
---|---|---|
Aluminio | 0.35 % Show Supplier Material materials with Aluminio of 0.35 % | max. |
Azufre | 0.015 % Show Supplier Material materials with Azufre of 0.015 % | max. |
Boro | 0.003 - 0.01 % Show Supplier Material materials with Boro of 0.003 - 0.01 % | |
Carbono | 0.08 % Show Supplier Material materials with Carbono of 0.08 % | max. |
Cromo | 13.5 - 16.0 % Show Supplier Material materials with Cromo of 13.5 - 16.0 % | |
Fósforo | 0.025 % Show Supplier Material materials with Fósforo of 0.025 % | max. |
Manganeso | 2.0 % Show Supplier Material materials with Manganeso of 2.0 % | max. |
Molibdeno | 1.0 - 1.8 % Show Supplier Material materials with Molibdeno of 1.0 - 1.8 % | |
Níquel | 24.0 - 27.0 % Show Supplier Material materials with Níquel of 24.0 - 27.0 % | |
Silicona | 1 % Show Supplier Material materials with Silicona of 1 % | max. |
Titanio | 1.9 - 2.3 % Show Supplier Material materials with Titanio of 1.9 - 2.3 % | |
Vanadio | 0.1 - 0.5 % Show Supplier Material materials with Vanadio of 0.1 - 0.5 % |
Technological properties
Property | ||
---|---|---|
Application areas | Power Generation, Connecting parts, Steam and gas turbine components like parts for mechanical systems, furnace construction, chemical and petrochemical industry and reactor technology | |
Processing history | Strain Hardened |