Medidas
Property | Value |
---|---|
Dimensions | Round-Bar length: 10.68-100 mm |
Mecánica
Property | Value |
---|---|
Resistencia a la tracción | 530.0 - 710.0 MPa Show Supplier Material materials with Resistencia a la tracción of 530.0 - 710.0 MPa |
Chemical properties
Property | Value | Comment |
---|---|---|
Azufre | 0.03 % Show Supplier Material materials with Azufre of 0.03 % | max. |
Boro | 0.05 - 0.1 % Show Supplier Material materials with Boro of 0.05 - 0.1 % | |
Carbono | 0.04 - 0.1 % Show Supplier Material materials with Carbono of 0.04 - 0.1 % | |
Cromo | 13.5 - 17.5 % Show Supplier Material materials with Cromo of 13.5 - 17.5 % | |
Fósforo | 0.045 % Show Supplier Material materials with Fósforo of 0.045 % | max. |
Manganeso | 1.5 % Show Supplier Material materials with Manganeso of 1.5 % | max. |
Molibdeno | 1.6 - 2.0 % Show Supplier Material materials with Molibdeno of 1.6 - 2.0 % | |
Niobio | 1.2 % Show Supplier Material materials with Niobio of 1.2 % | max. |
Níquel | 15.5 - 17.5 % Show Supplier Material materials with Níquel of 15.5 - 17.5 % | |
Silicona | 0.3 - 0.6 % Show Supplier Material materials with Silicona of 0.3 - 0.6 % |
Technological properties
Property | ||
---|---|---|
Application areas | Connecting parts, Mechanical Engineering, Components in machines and apparatus engineering, Cooling machine parts and similarly claimed parts for temperatures to -150°C | |
Processing history | Quenched and Tempered |