Medidas
Property | Value |
---|---|
Dimensions | Round-Bar length: 10.5-95 mm |
Chemical properties
Property | Value | Comment |
---|---|---|
Azufre | 0.035 % Show Supplier Material materials with Azufre of 0.035 % | max. |
Carbono | 0.14 - 0.19 % Show Supplier Material materials with Carbono of 0.14 - 0.19 % | |
Cromo | 1.4 - 1.7 % Show Supplier Material materials with Cromo of 1.4 - 1.7 % | |
Fósforo | 0.035 % Show Supplier Material materials with Fósforo of 0.035 % | max. |
Manganeso | 0.4 - 0.6 % Show Supplier Material materials with Manganeso of 0.4 - 0.6 % | |
Molibdeno | 5 % Show Supplier Material materials with Molibdeno of 5 % | max. |
Níquel | 1.4 - 1.7 % Show Supplier Material materials with Níquel of 1.4 - 1.7 % | |
Silicona | 0.4 % Show Supplier Material materials with Silicona of 0.4 % | max. |
Technological properties
Property | ||
---|---|---|
Application areas | Aerospace, Mechanical Engineering, Apparatus engineering | |
Processing history | Solution Annealed |