Medidas
Property | Value |
---|---|
Dimensions | Round-Bar length: 24.83-30.5 mm |
Mecánica
Property | Value |
---|---|
Resistencia a la tracción | 1040.0 - 1240.0 MPa Show Supplier Material materials with Resistencia a la tracción of 1040.0 - 1240.0 MPa |
Chemical properties
Property | Value | Comment |
---|---|---|
Azufre | 0.025 % Show Supplier Material materials with Azufre of 0.025 % | max. |
Carbono | 0.26 - 0.34 % Show Supplier Material materials with Carbono of 0.26 - 0.34 % | |
Cromo | 1.8 - 2.3 % Show Supplier Material materials with Cromo of 1.8 - 2.3 % | |
Fósforo | 0.025 % Show Supplier Material materials with Fósforo of 0.025 % | max. |
Manganeso | 0.3 - 0.6 % Show Supplier Material materials with Manganeso of 0.3 - 0.6 % | |
Molibdeno | 0.3 - 0.65 % Show Supplier Material materials with Molibdeno of 0.3 - 0.65 % | |
Níquel | 1.8 - 2.3 % Show Supplier Material materials with Níquel of 1.8 - 2.3 % | |
Silicona | 0.15 - 0.4 % Show Supplier Material materials with Silicona of 0.15 - 0.4 % |
Technological properties
Property | ||
---|---|---|
Application areas | Connecting parts, Mechanical Engineering | |
Processing history | Quenched and Tempered |