Medidas
Property | Value |
---|---|
Dimensions | Round-Bar length: 14.52-52.14 mm |
Mecánica
Property | Value | Comment |
---|---|---|
Elongación | 22 % Show Supplier Material materials with Elongación of 22 % | min. |
Límite elástico | 690.0 MPa Show Supplier Material materials with Límite elástico of 690.0 MPa | min., RP02 |
Resistencia a la tracción | 830.0 - 1080.0 MPa Show Supplier Material materials with Resistencia a la tracción of 830.0 - 1080.0 MPa |
Chemical properties
Property | Value | Comment |
---|---|---|
Aluminio | 0.02 - 0.05 % Show Supplier Material materials with Aluminio of 0.02 - 0.05 % | |
Azufre | 0.01 % Show Supplier Material materials with Azufre of 0.01 % | max. |
Carbono | 0.18 - 0.25 % Show Supplier Material materials with Carbono of 0.18 - 0.25 % | |
Cromo | 1.2 - 1.5 % Show Supplier Material materials with Cromo of 1.2 - 1.5 % | |
Fósforo | 0.02 % Show Supplier Material materials with Fósforo of 0.02 % | max. |
Manganeso | 0.3 - 0.5 % Show Supplier Material materials with Manganeso of 0.3 - 0.5 % | |
Molibdeno | 0.25 - 0.5 % Show Supplier Material materials with Molibdeno of 0.25 - 0.5 % | |
Níquel | 3.4 - 4.0 % Show Supplier Material materials with Níquel of 3.4 - 4.0 % | |
Silicona | 0.15 - 0.4 % Show Supplier Material materials with Silicona of 0.15 - 0.4 % |
Technological properties
Property | ||
---|---|---|
Application areas | Connecting parts | |
Processing history | Strain Hardened |