Medidas
Property | Value |
---|---|
Dimensions | Round-Bar length: 14.52-120 mm |
Chemical properties
Property | Value | Comment |
---|---|---|
Aluminio | 0.02 - 0.05 % Show Supplier Material materials with Aluminio of 0.02 - 0.05 % | |
Azufre | 0.015 % Show Supplier Material materials with Azufre of 0.015 % | max. |
Carbono | 0.25 - 0.3 % Show Supplier Material materials with Carbono of 0.25 - 0.3 % | |
Cromo | 1.2 - 1.7 % Show Supplier Material materials with Cromo of 1.2 - 1.7 % | |
Fósforo | 0.02 % Show Supplier Material materials with Fósforo of 0.02 % | max. |
Manganeso | 0.2 - 0.5 % Show Supplier Material materials with Manganeso of 0.2 - 0.5 % | |
Molibdeno | 0.35 - 0.55 % Show Supplier Material materials with Molibdeno of 0.35 - 0.55 % | |
Níquel | 3.3 - 3.8 % Show Supplier Material materials with Níquel of 3.3 - 3.8 % | |
Silicona | 0.3 % Show Supplier Material materials with Silicona of 0.3 % | max. |
Vanadio | 0.12 % Show Supplier Material materials with Vanadio of 0.12 % | max. |
Technological properties
Property | ||
---|---|---|
Application areas | Mechanical Engineering, Apparatus engineering | |
Processing history | Quenched and Tempered |