Medidas
Property | Value |
---|---|
Dimensions | Round-Bar length: 32 mm |
Chemical properties
Property | Value | Comment |
---|---|---|
Aluminio | 0.015 - 0.08 % Show Supplier Material materials with Aluminio of 0.015 - 0.08 % | |
Arsénico | 0.15 % Show Supplier Material materials with Arsénico of 0.15 % | max. |
Azufre | 002 % Show Supplier Material materials with Azufre of 002 % | max. |
Boro | 0.001 - 0.01 % Show Supplier Material materials with Boro of 0.001 - 0.01 % | |
Carbono | 0.17 - 0.23 % Show Supplier Material materials with Carbono of 0.17 - 0.23 % | |
Cobre | 0.2 % Show Supplier Material materials with Cobre of 0.2 % | max. |
Cromo | 0.9 - 1.2 % Show Supplier Material materials with Cromo of 0.9 - 1.2 % | |
Estaño | 0.02 % Show Supplier Material materials with Estaño of 0.02 % | max. |
Fósforo | 0.02 % Show Supplier Material materials with Fósforo of 0.02 % | max. |
Manganeso | 0.35 - 0.75 % Show Supplier Material materials with Manganeso of 0.35 - 0.75 % | |
Molibdeno | 0.9 - 1.1 % Show Supplier Material materials with Molibdeno of 0.9 - 1.1 % | |
Níquel | 0.2 % Show Supplier Material materials with Níquel of 0.2 % | max. |
Silicona | 0.4 % Show Supplier Material materials with Silicona of 0.4 % | max. |
Titanio | 0.07 - 0.15 % Show Supplier Material materials with Titanio of 0.07 - 0.15 % | |
Vanadio | 0.6 - 0.8 % Show Supplier Material materials with Vanadio of 0.6 - 0.8 % |
Technological properties
Property | ||
---|---|---|
Application areas | Aerospace, Defense Technology | |
Processing history | Quenched and Tempered |