Medidas
Property | Value |
---|---|
Dimensions | Round-Bar length: 14-120 mm - Sheet: 135x54-207x 54 mm |
Chemical properties
Property | Value | Comment |
---|---|---|
Azufre | 0.015 % Show Supplier Material materials with Azufre of 0.015 % | max. |
Carbono | 0.12 - 0.18 % Show Supplier Material materials with Carbono of 0.12 - 0.18 % | |
Cromo | 0.25 - 1.5 % Show Supplier Material materials with Cromo of 0.25 - 1.5 % | |
Fósforo | 0.02 % Show Supplier Material materials with Fósforo of 0.02 % | max. |
Manganeso | 0.8 - 1.0 % Show Supplier Material materials with Manganeso of 0.8 - 1.0 % | |
Molibdeno | 0.8 - 1.0 % Show Supplier Material materials with Molibdeno of 0.8 - 1.0 % | |
Silicona | 0.2 % Show Supplier Material materials with Silicona of 0.2 % | max. |
Vanadio | 0.2 - 0.3 % Show Supplier Material materials with Vanadio of 0.2 - 0.3 % |
Technological properties
Property | ||
---|---|---|
Application areas | Aerospace, Defense Technology | |
Processing history | Quenched and Tempered |