Medidas
Property | Value |
---|---|
Dimensions | Round-Bar length: 14-75 mm |
Chemical properties
Property | Value | Comment |
---|---|---|
Azufre | 0.025 % Show Supplier Material materials with Azufre of 0.025 % | |
Carbono | 0.2 % Show Supplier Material materials with Carbono of 0.2 % | max. |
Cerio | 0.45 % Show Supplier Material materials with Cerio of 0.45 % | max. |
Cobre | 0.55 % Show Supplier Material materials with Cobre of 0.55 % | max. |
Fósforo | 0.025 % Show Supplier Material materials with Fósforo of 0.025 % | max. |
Manganeso | 1.6 % Show Supplier Material materials with Manganeso of 1.6 % | max. |
Silicona | 0.55 % Show Supplier Material materials with Silicona of 0.55 % | max. |
Technological properties
Property | ||
---|---|---|
Application areas | Mechanical Engineering, Apparatus engineering | |
Processing history | Annealed and Forged |