Medidas
Property | Value |
---|---|
Dimensions | Round-Bar length: 16-65 mm |
Chemical properties
Property | Value | Comment |
---|---|---|
Azufre | 0.035 % Show Supplier Material materials with Azufre of 0.035 % | |
Carbono | 0.26 - 0.34 % Show Supplier Material materials with Carbono of 0.26 - 0.34 % | |
Cromo | 1.8 - 2.2 % Show Supplier Material materials with Cromo of 1.8 - 2.2 % | |
Fósforo | 0.025 % Show Supplier Material materials with Fósforo of 0.025 % | max. |
Manganeso | 0.3 - 0.6 % Show Supplier Material materials with Manganeso of 0.3 - 0.6 % | |
Molibdeno | 0.3 - 0.5 % Show Supplier Material materials with Molibdeno of 0.3 - 0.5 % | |
Níquel | 1.8 - 2.2 % Show Supplier Material materials with Níquel of 1.8 - 2.2 % | |
Silicona | 0.4 % Show Supplier Material materials with Silicona of 0.4 % | max. |
Technological properties
Property | ||
---|---|---|
Application areas | Mechanical Engineering, Tool technology, Automotive engineering | |
Processing history | Annealed and Forged |