Property | Value |
---|---|
Dimensions | Round-Bar length: 40-210 mm |
Mecánica
Property | Value | Comment |
---|---|---|
Elongación | 18 % Show Supplier Material materials with Elongación of 18 % | min. |
Límite elástico | 420.0 MPa Show Supplier Material materials with Límite elástico of 420.0 MPa | min., RP02 |
Resistencia a la tracción | 600.0 - 1100.0 MPa Show Supplier Material materials with Resistencia a la tracción of 600.0 - 1100.0 MPa |
Chemical properties
Property | Value | Comment |
---|---|---|
Azufre | 0.025 % Show Supplier Material materials with Azufre of 0.025 % | |
Carbono | 0.22 - 0.29 % Show Supplier Material materials with Carbono of 0.22 - 0.29 % | |
Cromo | 0.9 - 1.2 % Show Supplier Material materials with Cromo of 0.9 - 1.2 % | |
Fósforo | 0.03 % Show Supplier Material materials with Fósforo of 0.03 % | max. |
Manganeso | 0.5 - 0.8 % Show Supplier Material materials with Manganeso of 0.5 - 0.8 % | |
Molibdeno | 0.15 - 0.3 % Show Supplier Material materials with Molibdeno of 0.15 - 0.3 % | |
Silicona | 0.35 % Show Supplier Material materials with Silicona of 0.35 % | max. |
Technological properties
Property | ||
---|---|---|
Application areas | Mechanical Engineering, Tool technology, Automotive engineering, Aerospace | |
Processing history | Quenched and Tempered and Forged |