Medidas
Property | Value |
---|---|
Dimensions | Round-Bar length: 10-56 mm |
Mecánica
Property | Value | Comment |
---|---|---|
Dureza Brinell | 316.0 - 375.0 [-] Show Supplier Material materials with Dureza Brinell of 316.0 - 375.0 [-] | |
Elongación | 9 % Show Supplier Material materials with Elongación of 9 % | min. |
Límite elástico | 940.0 MPa Show Supplier Material materials with Límite elástico of 940.0 MPa | min., RP02 |
Resistencia a la tracción | 1040 MPa Show Supplier Material materials with Resistencia a la tracción of 1040 MPa | max. |
Chemical properties
Property | Value | Comment |
---|---|---|
Azufre | 0.02 - 0.035 % Show Supplier Material materials with Azufre of 0.02 - 0.035 % | |
Carbono | 0.38 - 0.45 % Show Supplier Material materials with Carbono of 0.38 - 0.45 % | |
Cromo | 0.9 - 1.2 % Show Supplier Material materials with Cromo of 0.9 - 1.2 % | |
Fósforo | 0.025 % Show Supplier Material materials with Fósforo of 0.025 % | max. |
Manganeso | 0.6 - 0.99 % Show Supplier Material materials with Manganeso of 0.6 - 0.99 % | |
Molibdeno | 0.15 - 0.3 % Show Supplier Material materials with Molibdeno of 0.15 - 0.3 % | |
Silicona | 0.4 % Show Supplier Material materials with Silicona of 0.4 % | max. |
Technological properties
Property | ||
---|---|---|
Application areas | Connecting parts, Mechanical Engineering, Automotive engineering | |
Processing history | Quenched and Tempered and Pealed |