Medidas
Property | Value |
---|---|
Dimensions | Round-Bar length: 20-120mm - Hexagonal Bar: 13- 24 mm |
Mecánica
Property | Value | Comment |
---|---|---|
Elongación | 10 % Show Supplier Material materials with Elongación of 10 % | min. |
Límite elástico | 500.0 MPa Show Supplier Material materials with Límite elástico of 500.0 MPa | min., RP02 |
Resistencia a la tracción | 650.0 - 1200.0 MPa Show Supplier Material materials with Resistencia a la tracción of 650.0 - 1200.0 MPa |
Chemical properties
Property | Value | Comment |
---|---|---|
Azufre | 0.02 - 0.035 % Show Supplier Material materials with Azufre of 0.02 - 0.035 % | |
Carbono | 0.38 - 0.45 % Show Supplier Material materials with Carbono of 0.38 - 0.45 % | |
Cromo | 0.9 - 1.2 % Show Supplier Material materials with Cromo of 0.9 - 1.2 % | |
Fósforo | 0.025 % Show Supplier Material materials with Fósforo of 0.025 % | max. |
Manganeso | 0.6 - 0.99 % Show Supplier Material materials with Manganeso of 0.6 - 0.99 % | |
Molibdeno | 0.15 - 0.3 % Show Supplier Material materials with Molibdeno of 0.15 - 0.3 % | |
Silicona | 0.4 % Show Supplier Material materials with Silicona of 0.4 % | max. |
Technological properties
Property | ||
---|---|---|
Application areas | Connecting parts, Mechanical Engineering, Automotive engineering | |
Processing history | Quenched and Tempered and Cold-drawn |