Medidas
Property | Value |
---|---|
Dimensions | Round-Bar length: 12-47 mm |
Chemical properties
Property | Value | Comment |
---|---|---|
Azufre | 0.02 - 0.035 % Show Supplier Material materials with Azufre of 0.02 - 0.035 % | |
Carbono | 0.38 - 0.45 % Show Supplier Material materials with Carbono of 0.38 - 0.45 % | |
Cromo | 0.9 - 1.2 % Show Supplier Material materials with Cromo of 0.9 - 1.2 % | |
Fósforo | 0.025 % Show Supplier Material materials with Fósforo of 0.025 % | max. |
Manganeso | 0.6 - 0.99 % Show Supplier Material materials with Manganeso of 0.6 - 0.99 % | |
Molibdeno | 0.15 - 0.3 % Show Supplier Material materials with Molibdeno of 0.15 - 0.3 % | |
Silicona | 0.4 % Show Supplier Material materials with Silicona of 0.4 % | max. |
Technological properties
Property | ||
---|---|---|
Application areas | Mechanical Engineering, Apparatus engineering, Connecting parts | |
Processing history | Annealed and Pealed |