Medidas
Property | Value |
---|---|
Dimensions | Round-Bar length: 36-220 mm |
Mecánica
Property | Value | Comment |
---|---|---|
Elongación | 16 % Show Supplier Material materials with Elongación of 16 % | min. |
Límite elástico | 550.0 MPa Show Supplier Material materials with Límite elástico of 550.0 MPa | min., RP02 |
Resistencia a la tracción | 700.0 - 850.0 MPa Show Supplier Material materials with Resistencia a la tracción of 700.0 - 850.0 MPa |
Chemical properties
Property | Value | Comment |
---|---|---|
Azufre | 0.03 % Show Supplier Material materials with Azufre of 0.03 % | |
Carbono | 0.17 - 0.25 % Show Supplier Material materials with Carbono of 0.17 - 0.25 % | |
Cromo | 1.2 - 1.5 % Show Supplier Material materials with Cromo of 1.2 - 1.5 % | |
Fósforo | 0.025 % Show Supplier Material materials with Fósforo of 0.025 % | max. |
Manganeso | 0.4 - 0.8 % Show Supplier Material materials with Manganeso of 0.4 - 0.8 % | |
Molibdeno | 0.55 - 0.8 % Show Supplier Material materials with Molibdeno of 0.55 - 0.8 % | |
Níquel | 0.6 % Show Supplier Material materials with Níquel of 0.6 % | max. |
Silicona | 0.4 % Show Supplier Material materials with Silicona of 0.4 % | max. |
Vanadio | 0.2 - 0.35 % Show Supplier Material materials with Vanadio of 0.2 - 0.35 % |
Technological properties
Property | ||
---|---|---|
Application areas | Mechanical Engineering, Apparatus engineering, Connecting parts | |
Processing history | Quenched and Tempered and Forged |