Medidas
Property | Value |
---|---|
Dimensions | Round-Bar length: 14-52 mm |
Chemical properties
Property | Value | Comment |
---|---|---|
Azufre | 0.03 % Show Supplier Material materials with Azufre of 0.03 % | |
Carbono | 0.17 - 0.25 % Show Supplier Material materials with Carbono of 0.17 - 0.25 % | |
Cromo | 1.2 - 1.5 % Show Supplier Material materials with Cromo of 1.2 - 1.5 % | |
Fósforo | 0.025 % Show Supplier Material materials with Fósforo of 0.025 % | max. |
Manganeso | 0.4 - 0.8 % Show Supplier Material materials with Manganeso of 0.4 - 0.8 % | |
Molibdeno | 0.55 - 0.8 % Show Supplier Material materials with Molibdeno of 0.55 - 0.8 % | |
Níquel | 0.6 % Show Supplier Material materials with Níquel of 0.6 % | max. |
Silicona | 0.4 % Show Supplier Material materials with Silicona of 0.4 % | max. |
Vanadio | 0.2 - 0.35 % Show Supplier Material materials with Vanadio of 0.2 - 0.35 % |
Technological properties
Property | ||
---|---|---|
Application areas | Mechanical Engineering, Apparatus engineering | |
Processing history | Annealed and Forged |