Medidas
Property | Value |
---|---|
Dimensions | Round-Bar length: 25-170 mm |
Mecánica
Property | Value | Comment |
---|---|---|
Elongación | 11 % Show Supplier Material materials with Elongación of 11 % | min. |
Límite elástico | 800.0 MPa Show Supplier Material materials with Límite elástico of 800.0 MPa | min., RP02 |
Resistencia a la tracción | 1250.0 - 1450.0 MPa Show Supplier Material materials with Resistencia a la tracción of 1250.0 - 1450.0 MPa |
Chemical properties
Property | Value | Comment |
---|---|---|
Aluminio | 0.015 % Show Supplier Material materials with Aluminio of 0.015 % | max. |
Azufre | 0.035 % Show Supplier Material materials with Azufre of 0.035 % | |
Carbono | 0.36 - 0.44 % Show Supplier Material materials with Carbono of 0.36 - 0.44 % | |
Cromo | 0.9 - 1.2 % Show Supplier Material materials with Cromo of 0.9 - 1.2 % | |
Fósforo | 0.03 % Show Supplier Material materials with Fósforo of 0.03 % | max. |
Manganeso | 0.35 - 0.85 % Show Supplier Material materials with Manganeso of 0.35 - 0.85 % | |
Molibdeno | 0.6 - 0.75 % Show Supplier Material materials with Molibdeno of 0.6 - 0.75 % | |
Silicona | 0.15 - 0.35 % Show Supplier Material materials with Silicona of 0.15 - 0.35 % | |
Vanadio | 0.25 - 0.35 % Show Supplier Material materials with Vanadio of 0.25 - 0.35 % |
Technological properties
Property | ||
---|---|---|
Application areas | Mechanical Engineering, Apparatus engineering, Connecting parts | |
Processing history | Quenched and Tempered and Forged |