Graphite CS31

Alternative and trade names
CS31
Want to keep this datasheet? Save it now in your required format

Description

GRAFSTARTM CS-31 carbon is ideal for specific customer applications requiring very high hardness, high strength, and very low thermal conductivity.

This material data has been provided by Advanced Graphite Materials.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyTemperatureValue

Density

23.0 °C

1.62 g/cm³

Show Supplier Material materials with Density of 1.62 g/cm³

Particle size range

0.76 µm

Show Supplier Material materials with Particle size range of 0.76 µm

Particle size

max.

Mechanical

PropertyTemperatureValue

Compressive strength

23.0 °C

35 MPa

Show Supplier Material materials with Compressive strength of 35 MPa

Flexural strength

23.0 °C

16 MPa

Show Supplier Material materials with Flexural strength of 16 MPa

Tensile strength

23.0 °C

12 MPa

Show Supplier Material materials with Tensile strength of 12 MPa

Thermal

PropertyTemperatureValue

Ash content

23.0 °C

0.2 %

Show Supplier Material materials with Ash content of 0.2 %

Thermal conductivity, in-plane

23.0 °C

10 W/(m·K)

Show Supplier Material materials with Thermal conductivity, in-plane of 10 W/(m·K)

Electrical

PropertyTemperatureValue

Electrical resistivity

23.0 °C

4.19E-5 Ω·m

Show Supplier Material materials with Electrical resistivity of 4.19E-5 Ω·m

Electrical resistivity, transverse

23.0 °C

5E-5 Ω·m

Show Supplier Material materials with Electrical resistivity, transverse of 5E-5 Ω·m

Technological properties

Property
Application areas

Anodes for electrolytic processes, Applications that require low thermal conductivity material