Graphite TS5328

Want to keep this datasheet? Save it now in your required format

Description

TS5328 graphite is a fine grain, high strength material that can be machined to precise tolerances and a fine surface finish. It has a unique thermal shock resistance due to the combination of low thermal expansion, high thermal conductivity and low elastic modulus

This material data has been provided by Advanced Graphite Materials.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValue

Density

23.0 °C

1.74 g/cm³

Show Supplier Material materials with Density of 1.74 g/cm³

Mechanical

PropertyTemperatureValue

Compressive strength

23.0 °C

65 MPa

Show Supplier Material materials with Compressive strength of 65 MPa

Elastic modulus

23.0 °C

9.5 GPa

Show Supplier Material materials with Elastic modulus of 9.5 GPa

Flexural strength

23.0 °C

40 MPa

Show Supplier Material materials with Flexural strength of 40 MPa

Hardness, Rockwell L

23.0 °C

68 [-]

Show Supplier Material materials with Hardness, Rockwell L of 68 [-]

Tensile strength

23.0 °C

24 MPa

Show Supplier Material materials with Tensile strength of 24 MPa

Thermal

PropertyTemperatureValueComment

Ash content

23.0 °C

0.5 %

Show Supplier Material materials with Ash content of 0.5 %

For applications requiring low ash, a purified version of this grade is available

Coefficient of thermal expansion

23.0 °C

3.8E-6 1/K

Show Supplier Material materials with Coefficient of thermal expansion of 3.8E-6 1/K

average for 20-100°C

Thermal conductivity, in-plane

23.0 °C

120 W/(m·K)

Show Supplier Material materials with Thermal conductivity, in-plane of 120 W/(m·K)

Electrical

PropertyTemperatureValue

Electrical resistivity

23.0 °C

1.15E-5 Ω·m

Show Supplier Material materials with Electrical resistivity of 1.15E-5 Ω·m

Technological properties

Property
Application areas

Permanent molds, Composite tooling, Continuous casting dies, Hot pressing molds and punches, Rocket motor nozzles, Plunger and rams