Graphite DBX

Want to keep this datasheet? Save it now in your required format

Description

High thermal shock resistance, Strength increases with temperature, Performs at high temperatures, Superior oxidation resistance

This material data has been provided by Advanced Graphite Materials.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValue

Density

23.0 °C

1.73 g/cm³

Show Supplier Material materials with Density of 1.73 g/cm³

Particle size range

0.76 µm

Show Supplier Material materials with Particle size range of 0.76 µm

Porosity

14 %

Show Supplier Material materials with Porosity of 14 %

Particle size

max.

Mechanical

PropertyTemperatureValue

Compressive strength

23.0 °C

46 MPa

Show Supplier Material materials with Compressive strength of 46 MPa

Compressive strength, transverse

23.0 °C

46 MPa

Show Supplier Material materials with Compressive strength, transverse of 46 MPa

Elastic modulus

23.0 °C

10 GPa

Show Supplier Material materials with Elastic modulus of 10 GPa

Elastic modulus, transverse

23.0 °C

8.9 GPa

Show Supplier Material materials with Elastic modulus, transverse of 8.9 GPa

Flexural strength

23.0 °C

22 MPa

Show Supplier Material materials with Flexural strength of 22 MPa

Flexural strength, transverse

23.0 °C

16 MPa

Show Supplier Material materials with Flexural strength, transverse of 16 MPa

Tensile strength

23.0 °C

15 MPa

Show Supplier Material materials with Tensile strength of 15 MPa

Tensile strength, transverse

23.0 °C

12 MPa

Show Supplier Material materials with Tensile strength, transverse of 12 MPa

Thermal

PropertyTemperatureValueComment

Ash content

23.0 °C

0.12 %

Show Supplier Material materials with Ash content of 0.12 %

Coefficient of thermal expansion

23.0 °C

2.5E-6 1/K

Show Supplier Material materials with Coefficient of thermal expansion of 2.5E-6 1/K

average for 20-100°C

Coefficient of thermal expansion, transverse

23.0 °C

3.5E-6 1/K

Show Supplier Material materials with Coefficient of thermal expansion, transverse of 3.5E-6 1/K

average for 20-100°C

Thermal conductivity, in-plane

23.0 °C

175 W/(m·K)

Show Supplier Material materials with Thermal conductivity, in-plane of 175 W/(m·K)

Thermal conductivity, through-plane

23.0 °C

150 W/(m·K)

Show Supplier Material materials with Thermal conductivity, through-plane of 150 W/(m·K)

Electrical

PropertyTemperatureValue

Electrical resistivity

23.0 °C

6.5E-6 Ω·m

Show Supplier Material materials with Electrical resistivity of 6.5E-6 Ω·m

Electrical resistivity, transverse

23.0 °C

9E-6 Ω·m

Show Supplier Material materials with Electrical resistivity, transverse of 9E-6 Ω·m

Technological properties

Property
Application areas

Diamond Drill Bit Mold Material