CEN/TS 13388 Grade CW117C R250, H060

Want to keep this datasheet? Save it now in your required format

Related Standards

This material data has been provided by AluKey.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValue

Density

20.0 °C

8.9 g/cm³

Show Material materials with Density of 8.9 g/cm³

Dimension

PropertyValue

Dimensions

Dicke

Mechanical

PropertyTemperatureValue

Elastic modulus

20.0 °C

120 GPa

Show Material materials with Elastic modulus of 120 GPa

Elongation A50

20.0 °C

9 %

Show Material materials with Elongation A50 of 9 %

Hardness, Vickers

20.0 °C

60 - 90 [-]

Show Material materials with Hardness, Vickers of 60 - 90 [-]

Tensile strength

20.0 °C

250 - 320 MPa

Show Material materials with Tensile strength of 250 - 320 MPa

Yield strength Rp0.2

20.0 °C

200 MPa

Show Material materials with Yield strength Rp0.2 of 200 MPa

Thermal

PropertyTemperatureValue

Coefficient of thermal expansion

20.0 °C

1.73E-5 1/K

Show Material materials with Coefficient of thermal expansion of 1.73E-5 1/K

100.0 °C

1.73E-5 1/K

Show Material materials with Coefficient of thermal expansion of 1.73E-5 1/K

Melting point

1081 °C

Show Material materials with Melting point of 1081 °C

Specific heat capacity

20.0 °C

385 J/(kg·K)

Show Material materials with Specific heat capacity of 385 J/(kg·K)

Thermal conductivity

20.0 °C

340 W/(m·K)

Show Material materials with Thermal conductivity of 340 W/(m·K)

Electrical

PropertyTemperatureValue

Electrical conductivity

20.0 °C

4.70E+7 S/m

Show Material materials with Electrical conductivity of 4.70E+7 S/m

Electrical resistivity

20.0 °C

2.13E-8 Ω·m

Show Material materials with Electrical resistivity of 2.13E-8 Ω·m

Chemical properties

PropertyValue

Iron

0.02 %

Show Material materials with Iron of 0.02 %

Nickel

0.02 %

Show Material materials with Nickel of 0.02 %

Other

Rest Cu, total 0.1

Phosphorus

0.02 %

Show Material materials with Phosphorus of 0.02 %

Tin

0.1 - 0.15 %

Show Material materials with Tin of 0.1 - 0.15 %

Zinc

0.1 %

Show Material materials with Zinc of 0.1 %

Technological properties

Property
Brazing

hard brazing : very good to good, soft brazing: very good to good

Workability

Cold forming degree between anneals: max. 95 %, general (condition): very good