Properties

General

PropertyTemperatureValue

Density

20.0 °C

8.4 g/cm³

Show Material materials with Density of 8.4 g/cm³

Dimension

PropertyValue

Dimensions

Durchmesser

Mechanical

PropertyTemperatureValue

Elongation

20.0 °C

5 %

Show Material materials with Elongation of 5 %

Hardness, Brinell

20.0 °C

130 [-]

Show Material materials with Hardness, Brinell of 130 [-]

Hardness, Vickers

20.0 °C

135 [-]

Show Material materials with Hardness, Vickers of 135 [-]

Tensile strength

20.0 °C

480 MPa

Show Material materials with Tensile strength of 480 MPa

Yield strength Rp0.2

20.0 °C

330 MPa

Show Material materials with Yield strength Rp0.2 of 330 MPa

Chemical properties

PropertyValue

Copper

55 - 57 %

Show Material materials with Copper of 55 - 57 %

Iron

0.3 %

Show Material materials with Iron of 0.3 %

Lead

1.6 - 3 %

Show Material materials with Lead of 1.6 - 3 %

Nickel

0.3 %

Show Material materials with Nickel of 0.3 %

Other

Rest Zn, total 0.2

Tin

0.3 %