AMPCO® 25 Continuous cast

Want to keep this datasheet? Save it now in your required format

Description

AMPCO® 25 is a patented alloy which displays outstanding mechanical properties. The extreme hardness, linked with an excellent compressive strength and very good friction properties, makes it ideal as a forming and drawing die material. As the elongation of the material is nil, thin sections should be avoided and the material should be well backed up.

This material data has been provided by AMPCO METAL.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyValueTemperature

Density

6.93 g/cm³

Show Supplier Material materials with Density of 6.93 g/cm³ at 23.0 °C

23.0 °C

Mechanical

PropertyValueTemperatureComment

Compressive strength

1551 MPa

Show Supplier Material materials with Compressive strength of 1551 MPa at 23.0 °C

23.0 °C

Compressive yield strength, 0.1%

689 MPa

Show Supplier Material materials with Compressive yield strength, 0.1% of 689 MPa at 23.0 °C

23.0 °C

Elastic modulus

110 GPa

Show Supplier Material materials with Elastic modulus of 110 GPa at 23.0 °C

23.0 °C

Hardness, HBW

364 [-]

Show Supplier Material materials with Hardness, HBW of 364 [-] at 23.0 °C

23.0 °C

HBW 10/3000

Hardness, Rockwell C

38 [-]

Show Supplier Material materials with Hardness, Rockwell C of 38 [-] at 23.0 °C

23.0 °C

Thermal

PropertyValueTemperature

Coefficient of thermal expansion

1.62E-5 1/K

Show Supplier Material materials with Coefficient of thermal expansion of 1.62E-5 1/K at 23.0 °C

23.0 °C

Specific heat capacity

420 J/(kg·K)

Show Supplier Material materials with Specific heat capacity of 420 J/(kg·K) at 23.0 °C

23.0 °C

Thermal conductivity

33 W/(m·K)

Show Supplier Material materials with Thermal conductivity of 33 W/(m·K) at 23.0 °C

23.0 °C

Electrical

PropertyValueTemperature

Electrical conductivity

4.00E+6 S/m

Show Supplier Material materials with Electrical conductivity of 4.00E+6 S/m at 23.0 °C

23.0 °C

Specific Electrical conductivity

8 % IACS

Show Supplier Material materials with Specific Electrical conductivity of 8 % IACS

Chemical properties

Property

Copper

Balance

Technological properties

Property
Application areas

The phenomenal success of this alloy led to its use as forming rolls, bending and wiping blocks and it is considered the standard material in this field of applications. Due to its inherent friction properties, this alloy has an excellent behaviour in any wear application where high compression loads are present.