General
Property | Temperature | Value |
---|---|---|
Density | 23.0 °C | 6.84 g/cm³ Show Supplier Material materials with Density of 6.84 g/cm³ |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Compressive strength | 23.0 °C | 1608 MPa Show Supplier Material materials with Compressive strength of 1608 MPa | |
Compressive yield strength, 0.1% | 23.0 °C | 715 MPa Show Supplier Material materials with Compressive yield strength, 0.1% of 715 MPa | |
Hardness, HBW | 23.0 °C | 420 [-] Show Supplier Material materials with Hardness, HBW of 420 [-] | HBW 10/3000 |
Hardness, Rockwell C | 23.0 °C | 44 [-] Show Supplier Material materials with Hardness, Rockwell C of 44 [-] |
Thermal
Property | Temperature | Value |
---|---|---|
Coefficient of thermal expansion | 23.0 °C | 1.6E-5 1/K Show Supplier Material materials with Coefficient of thermal expansion of 1.6E-5 1/K |
Specific heat capacity | 23.0 °C | 420 J/(kg·K) Show Supplier Material materials with Specific heat capacity of 420 J/(kg·K) |
Thermal conductivity | 23.0 °C | 33 W/(m·K) Show Supplier Material materials with Thermal conductivity of 33 W/(m·K) |
Electrical
Property | Temperature | Value |
---|---|---|
Electrical conductivity | 23.0 °C | 4.00E+6 S/m Show Supplier Material materials with Electrical conductivity of 4.00E+6 S/m |
Specific Electrical conductivity | 8 % IACS Show Supplier Material materials with Specific Electrical conductivity of 8 % IACS |
Chemical properties
Property | Value |
---|---|
Copper | Balance |
Technological properties
Property | ||
---|---|---|
Application areas | Stainless steel drawing dies, forming rolls under great stresses and extreme pressures are the most typical applications for this alloy. |