Kepstan® 8002

Alternative and trade names
PEKK
Want to keep this datasheet? Save it now in your required format

Description

KEPSTAN® PEKK resin is a high performance thermoplastic material, based on PolyEtherKetoneKetone (PEKK) highly stable chemical backbone. Its semi crystalline structure in solid state offers an outstanding combination of mechanical and thermal strength together with chemical and fire resistance.

The 8000 Series offers the highest glass transition temperature and the highest degree of crystallinity, leading to the best tensile and compression strengths among the wide range of PEKK copolymers within the KEPSTAN® product range.

KEPSTAN® 8000 Series includes a low flow grade, KEPSTAN® 8001, and a medium flow grade, KEPSTAN® 8002, both unfilled pure PEKK resins designed to meet the requirements of a broad range of melt processing technologies, including among others extrusion of stock shapes, tubes, films, extrusion compression, compression molding, injection molding of thick or complex and thin-walled parts.

KEPSTAN® PEKK resin is available in pellet form and in powder form with different particle sizes. Standard packaging includes 20 kg boxes for pellets and 10 kg boxes for powders.

This material data has been provided by Arkema High Performance Polymers.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

1.29 g/cm³

Show Supplier Material materials with Density of 1.29 g/cm³

ISO 1183

Limiting oxygen index

23.0 °C

35 %

Show Supplier Material materials with Limiting oxygen index of 35 %

ISO 4589-1/-2

Mechanical

PropertyTemperatureValueComment

Elastic modulus

23.0 °C

3.8 GPa

Show Supplier Material materials with Elastic modulus of 3.8 GPa

ISO 527-1/-2

Impact strength, Charpy notched

-30.0 °C

4.5 kJ/m²

Show Supplier Material materials with Impact strength, Charpy notched of 4.5 kJ/m²

ISO 179/1eA

23.0 °C

4.5 kJ/m²

Show Supplier Material materials with Impact strength, Charpy notched of 4.5 kJ/m²

ISO 179/1eA

Impact strength, Charpy unnotched

-30.0 °C

40 kJ/m²

Show Supplier Material materials with Impact strength, Charpy unnotched of 40 kJ/m²

ISO 179/1eU

23.0 °C

62 kJ/m²

Show Supplier Material materials with Impact strength, Charpy unnotched of 62 kJ/m²

ISO 179/1eU

Unlock all property charts

Thermal

PropertyValueComment

Heat deflection temperature, 1.80 MPa

175 °C

Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 175 °C

ISO 75-1/-2

Electrical

PropertyTemperatureValueComment

Dielectric constant, 1MHz

23.0 °C

2.6 [-]

Show Supplier Material materials with Dielectric constant, 1MHz of 2.6 [-]

IEC 60250

Rheological Properties

PropertyValueComment

Melt volume-flow rate

35 cm³/10min

Show Supplier Material materials with Melt volume-flow rate of 35 cm³/10min

ISO 1133, 380°C/5kg

Technological properties

Property
Application areas

Connectors,Fittings, Components, and Injection Molded Parts,Cable Ties,Chemical Process Industry,Chemical Process Industry - Coating of Chemical Pumps,Chemical Process Industry - Coating of Chemical Valves,Chemical Process Industry - Coating of Chemical Vessels,Chemical Process Industry - High Purity Piping,Chemical Process Industry - Injection Molding,Monofilaments,Powder Coatings - Wire Goods,Connectors E&E,Performance Wire,Wire and Cables,Natural Gas Distribution- Fittings

Processing methods

Injection Molding:

  • Drying temperature and time: 150°C for 3 to 4 hours or 120°C for 6 to 8 hours
  • Processing temperature: 375 – 385°C
  • Temperature settings - Injection: Rear 350°C / Center 375°C / Front 375°C / Nozzle 385°C
  • Mold temperature (to facilitate filling of the cavity and polymer crystallization): 220 - 240°C
  • Temperature settings - Extrusion Zones 1/2/3/4: 340°C/ 360°C/ 380°C/ 380°C Die: 370°C