KEPSTAN® PEKK resin is a high performance thermoplastic material, based on PolyEtherKetoneKetone (PEKK) highly stable chemical backbone. Its semi crystalline structure in solid state offers an outstanding combination of mechanical and thermal strength together with chemical and fire resistance. KEPSTAN® 8010C30 is a carbon fiber reinforced compound, based on the 8000 series of KEPSTAN® resins. This series offers the highest glass transition temperature and the highest crystallinity, leading to the best tensile and compression strengths among the different series of KEPSTAN® PEKK copolymers.

KEPSTAN® 8010C30 is a low flow grade, suitable for extrusion, compression and injection molding.

KEPSTAN® 8010C30 is available in pellet form, and standard packaging is 10 kg boxes.

This material data has been provided by Arkema High Performance Polymers.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

1.45 g/cm³

Show Supplier Material materials with Density of 1.45 g/cm³

ISO 1183

Mechanical

PropertyTemperatureValueComment

Impact strength, Charpy notched

23.0 °C

6 kJ/m²

Show Supplier Material materials with Impact strength, Charpy notched of 6 kJ/m²

ISO 179/1eA

Impact strength, Charpy unnotched

23.0 °C

34 kJ/m²

Show Supplier Material materials with Impact strength, Charpy unnotched of 34 kJ/m²

ISO 179/1eU

Rheological Properties

PropertyValueComment

Melt volume-flow rate

18 cm³/10min

Show Supplier Material materials with Melt volume-flow rate of 18 cm³/10min

ISO 1133, 380°C/5kg

Technological properties

Property
Application areas

Fittings, Components, and Injection Molded Parts,Chemical Process Industry,Chemical Process Industry - Injection Molding,Chemical Process Industry - Stock Shapes

Fillers

40% Carbon Fiber

Processing methods

Injection Molding:

  • Drying temperature and time: 120°C for 6 to 8 hours
  • Processing temperature: 370 – 380°C
  • Temperature settings - Injection: Rear 350°C / Center 375°C / Front 370°C / Nozzle 385°C
  • Mold temperature (to facilitate filling of the cavity and polymer crystallization): 230 - 240°C
  • Temperature settings - Extrusion Zones 1/2/3/4: 355°C/ 370°C/ 385°C/ 385°C Die: 370°C