Kepstan® 8010G30

Alternative and trade names
PEKK-GF30
Want to keep this datasheet? Save it now in your required format

Description

KEPSTAN® PEKK resin is a high performance thermoplastic material, based on PolyEtherKetoneKetone (PEKK) highly stable chemical backbone. KEPSTAN® is a unique member of the PAEK family that incorporates distinctive structural features that allow for exceptional possibilities in the control of crystallinity. These features include a low Ether/Ketone ratio and a copolymer structure incorporating Terephthalic and Isophthalic moieties.

KEPSTAN® 8010G30 resin is a glass fiber reinforced compound, based on the 8000 series of KEPSTAN® resins. This series offers the highest glass transition temperature and the highest crystallinity, leading to the best tensile and compression strengths among the different series of KEPSTAN® PEKK copolymers.

KEPSTAN® 8010G30 resin is a low flow grade, suitable for extrusion, compression and injection molding.

KEPSTAN® 8010G30 resin is available in pellet form and standard packaging is 10 kg boxes.

This material data has been provided by Arkema High Performance Polymers.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

1.52 g/cm³

Show Supplier Material materials with Density of 1.52 g/cm³

ISO 1183

Rheological Properties

PropertyValueComment

Melt volume-flow rate

7 cm³/10min

Show Supplier Material materials with Melt volume-flow rate of 7 cm³/10min

ISO 1133, 380°C/5kg

Technological properties

Property
Application areas

Connectors,Fittings, Components, and Injection Molded Parts,Chemical Process Industry,Chemical Process Industry - Injection Molding,Chemical Process Industry - Stock Shapes,Connectors E&E

Fillers

30% Glass Fiber

Processing methods

Injection Molding:

  • Drying temperature and time: 150°C for 3 to 4 hours or 120°C for 6 to 8 hours
  • Processing temperature: 375 – 385°C
  • Temperature settings - Injection: Rear 350°C / Center 375°C / Front 375°C / Nozzle 385°C
  • Mold temperature (to facilitate filling of the cavity and polymer crystallization): 230 - 240°C
  • Temperature settings - Extrusion Zones 1/2/3/4: 355°C/ 370°C/ 385°C/ 385°C Die: 370°C