Kynar Flex® 2850-02

Alternative and trade names
PVDF
Want to keep this datasheet? Save it now in your required format

Description

Kynar Flex® resins are fluorinated thermoplastic copolymers.

Kynar Flex® 2850-02 has been specifically designed for use in wire and cable constructions which require an Underwriters Laboratories temperature of 150ºC and a Limiting Oxygen Index (LOI) of at least 75.

Kynar Flex® 2850-02 is easily processed and has excellent physical, mechanical, thermal and flame resistant characteristics.

Kynar Flex® 2850-02 meets the smoke and flame requirements of UL 910 and ASTM E84 (the Modified Steiner Tunnel Test). This copolymer is commonly used for pipe, wire jacketing, conduits, and in injection molded parts. ADDITIONAL CHARACTERISTICS:

  • Excellent thermal stability
  • Excellent abrasion resistance
  • Impervious to UV degradation
  • Self extinguishing material
  • Extremely low smoke emission characteristics
  • 0/0 rating in ASTM E-84/UL 723

  • This material data has been provided by Arkema High Performance Polymers.

    All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
    Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

    Ashby charts

    Properties

    General

    PropertyTemperatureValueComment

    Density

    23.0 °C

    1.77 - 1.8 g/cm³

    Show Supplier Material materials with Density of 1.77 - 1.8 g/cm³

    ASTM D792

    Mechanical

    PropertyTemperatureValueComment

    Compressive strength

    23.0 °C

    41.4 - 58.6 MPa

    Show Supplier Material materials with Compressive strength of 41.4 - 58.6 MPa

    ASTM D695

    Elongation

    23.0 °C

    30 - 200 %

    Show Supplier Material materials with Elongation of 30 - 200 %

    ASTM D638

    Flexural modulus

    23.0 °C

    1.03 - 1.24 GPa

    Show Supplier Material materials with Flexural modulus of 1.03 - 1.24 GPa

    ASTM D790

    Hardness, Shore D

    23.0 °C

    70 - 75 [-]

    Show Supplier Material materials with Hardness, Shore D of 70 - 75 [-]

    ASTM D2240

    Tensile strength

    23.0 °C

    27.6 - 48.3 MPa

    Show Supplier Material materials with Tensile strength of 27.6 - 48.3 MPa

    ASTM D638

    Yield strength

    23.0 °C

    31 - 41.4 MPa

    Show Supplier Material materials with Yield strength of 31 - 41.4 MPa

    ASTM D638

    Thermal

    PropertyValueComment

    Melting point

    155 - 160 °C

    Show Supplier Material materials with Melting point of 155 - 160 °C

    ASTM D3418

    Electrical

    PropertyTemperatureValueComment

    Volume resistivity

    23.0 °C

    2.00E+14 Ω·cm

    Show Supplier Material materials with Volume resistivity of 2.00E+14 Ω·cm

    ASTM D257, 65% RH

    Rheological Properties

    PropertyTemperatureValueComment

    Melt viscosity

    23.0 °C

    2300 - 2700 Pa·s

    Show Supplier Material materials with Melt viscosity of 2300 - 2700 Pa·s

    ASTM D3835

    Technological properties

    Property
    Application areas

    Plenum Pipe,Wire and Cables