Kynar Flex® 3030-10

Alternative and trade names
PVDF
Want to keep this datasheet? Save it now in your required format

Description

Kynar Flex® resins are fluorinated thermoplastic copolymers.

This material data has been provided by Arkema Technical Polymers.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyValueTesting StandardConditionComment

Density

1.78 - 1.82 g/cm³

Show Supplier Material materials with Density of 1.78 - 1.82 g/cm³

ASTM D792

Limiting oxygen index

42 %

Show Supplier Material materials with Limiting oxygen index of 42 %

ASTM D2863

45 %

Show Supplier Material materials with Limiting oxygen index of 45 %

ISO 4589-1/-2

dry

Water absorption

0.5 %

Show Supplier Material materials with Water absorption of 0.5 %

ASTM D570

max.

Mechanical

PropertyValueTesting StandardConditionComment

Elastic modulus

0.207 - 0.345 GPa

Show Supplier Material materials with Elastic modulus of 0.207 - 0.345 GPa

ASTM D638

0.283 GPa

Show Supplier Material materials with Elastic modulus of 0.283 GPa

ISO 527-1/-2

dry

Elongation

50 %

Show Supplier Material materials with Elongation of 50 %

ISO 527-1/-2

dry

min. | nominal

500 %

Show Supplier Material materials with Elongation of 500 %

ASTM D638

min.

Elongation at yield

25 - 40 %

Show Supplier Material materials with Elongation at yield of 25 - 40 %

ASTM D638

30 %

Show Supplier Material materials with Elongation at yield of 30 %

ISO 527-1/-2

dry

Flexural modulus

0.241 - 0.379 GPa

Show Supplier Material materials with Flexural modulus of 0.241 - 0.379 GPa

ASTM D790

Hardness, Shore D

45 - 55 [-]

Show Supplier Material materials with Hardness, Shore D of 45 - 55 [-]

ASTM D2240

Impact strength, Charpy notched

No Break at 23°C

ISO 179/1eA

dry

Impact strength, Charpy notched, ASTM

No Break at 23°C

ASTM D256

Tensile strength

19.3 - 24.8 MPa

Show Supplier Material materials with Tensile strength of 19.3 - 24.8 MPa

ASTM D638

Yield strength

12.4 - 16.5 MPa

Show Supplier Material materials with Yield strength of 12.4 - 16.5 MPa

ASTM D638

Thermal

PropertyValueTesting StandardConditionComment

Coefficient of thermal expansion

0.000153 - 0.000194 1/K

Show Supplier Material materials with Coefficient of thermal expansion of 0.000153 - 0.000194 1/K

ASTM D696

Glass transition temperature

-42 °C

Show Supplier Material materials with Glass transition temperature of -42 °C

ISO 11357-1/-2

dry

10°C/min

-40 °C

Show Supplier Material materials with Glass transition temperature of -40 °C

ASTM D7028

Melting point

160 - 168 °C

Show Supplier Material materials with Melting point of 160 - 168 °C

ASTM D3418

164 °C

Show Supplier Material materials with Melting point of 164 °C

ISO 11357-1/-3

dry

10°C/min

Flammability

At thickness 0.8 mm IEC 60695-11-10: V-0

Electrical

PropertyValueTesting StandardCondition

Dielectric strength

39.4 - 47.2 kV/mm

Show Supplier Material materials with Dielectric strength of 39.4 - 47.2 kV/mm

ASTM D149

Surface resistivity

7.6e+11 - 7.8e+11 Ω/sq

Show Supplier Material materials with Surface resistivity of 7.6e+11 - 7.8e+11 Ω/sq

ASTM D257

Volume resistivity

2e+14 Ω·cm

Show Supplier Material materials with Volume resistivity of 2e+14 Ω·cm

IEC 60093

dry

Rheological Properties

PropertyValueTesting StandardComment

Melt mass-flow rate

8 - 25 g/10min

Show Supplier Material materials with Melt mass-flow rate of 8 - 25 g/10min

ASTM D1238

230°C/3.8kg

Melt viscosity

700 - 1300 Pa·s

Show Supplier Material materials with Melt viscosity of 700 - 1300 Pa·s

ASTM D3835

Technological properties

Property
Application areas

Automotive Cables,Foamed PVDF Cable Jacketing,Performance Wire,PVDF Cable Jacketing,Wire and Cables