Kynar Flex® PPA 2200

Alternative and trade names
PVDF
Want to keep this datasheet? Save it now in your required format

Description

Kynar Flex® resins are fluorinated thermoplastic copolymers.

Kynar Flex® PPA 2200 resin is specially designed pellet used as a polymer process aid (PPA) for polyolefins. The use of Kynar Flex® PPA 2200 resin at 200-1000 ppm levels reduces extruder pressure, improves surface finish, reduces die build up, and improves gauge control.

This material data has been provided by Arkema High Performance Polymers.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyTemperatureValueComment

Bulk density

23.0 °C

0.6 - 0.8 g/cm³

Show Supplier Material materials with Bulk density of 0.6 - 0.8 g/cm³

MOD-SRDP/POU-084

Density

23.0 °C

0.7 g/cm³

Show Supplier Material materials with Density of 0.7 g/cm³

ISO 1183

Thermal

PropertyValueComment

Melting point

144 °C

Show Supplier Material materials with Melting point of 144 °C

ISO 11357-1/-3, 10°C/min