Kynar Flex® PPA 8600

Alternative and trade names
PVDF
Want to keep this datasheet? Save it now in your required format

Description

Kynar Flex® resins are fluorinated thermoplastic copolymers.

Kynar Flex® PPA 8600 resin is specially designed pellet used as a polymer process aid (PPA) for polyolefins. The use of Kynar Flex® PPA 8600 resin at 200-1000 ppm levels reduces extruder pressure, improves surface finish, reduces die build up, and improves gauge control. This product is also available on a powder form as Kynar Flex® PPA 8601 resin.

This material data has been provided by Arkema High Performance Polymers.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyTemperatureValueComment

Bulk density

23.0 °C

0.5 - 0.9 g/cm³

Show Supplier Material materials with Bulk density of 0.5 - 0.9 g/cm³

MOD-SRDP/POU-084

Density

23.0 °C

0.7 g/cm³

Show Supplier Material materials with Density of 0.7 g/cm³

ISO 1183

Thermal

PropertyValueComment

Glass transition temperature

-40 °C

Show Supplier Material materials with Glass transition temperature of -40 °C

ISO 11357-1/-2, 10°C/min

Melting point

165 °C

Show Supplier Material materials with Melting point of 165 °C

ISO 11357-1/-3, 10°C/min

Technological properties

Property
Application areas

Fluoropolymer Processing Aids