Description

Kynar® resins are fluorinated thermoplastic homopolymers.

Kynar® 340 resin is a thermoplastic fluorinated polymer resin. The properties are the same as standard grade: chemical resistance, resistance to UV, low permeation, high purity, excellent mechanical behavior. More over, this grade is electrically conductive. This grade is available as pellet form for injection, extrusion, compression.

This material data has been provided by Arkema High Performance Polymers.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

1.78 g/cm³

Show Supplier Material materials with Density of 1.78 g/cm³

ISO 1183

Limiting oxygen index

23.0 °C

43 %

Show Supplier Material materials with Limiting oxygen index of 43 %

ISO 4589-1/-2

Mechanical

PropertyTemperatureValueComment

Elastic modulus

23.0 °C

1.6 GPa

Show Supplier Material materials with Elastic modulus of 1.6 GPa

ISO 527-1/-2

Elongation

23.0 °C

40 %

Show Supplier Material materials with Elongation of 40 %

min., ISO 527-1/-2, nominal

Elongation at yield

23.0 °C

5 %

Show Supplier Material materials with Elongation at yield of 5 %

ISO 527-1/-2

Impact strength, Charpy notched

-30.0 °C

5 kJ/m²

Show Supplier Material materials with Impact strength, Charpy notched of 5 kJ/m²

ISO 179/1eA

23.0 °C

9 kJ/m²

Show Supplier Material materials with Impact strength, Charpy notched of 9 kJ/m²

ISO 179/1eA

Yield strength

23.0 °C

10 MPa

Show Supplier Material materials with Yield strength of 10 MPa

ISO 527-1/-2

Thermal

PropertyValueComment

Melting point

166 °C

Show Supplier Material materials with Melting point of 166 °C

ISO 11357-1/-3, 10°C/min

Electrical

PropertyTemperatureValueComment

Dielectric constant, 100Hz

23.0 °C

0.07 [-]

Show Supplier Material materials with Dielectric constant, 100Hz of 0.07 [-]

IEC 60250

Dielectric strength

23.0 °C

27 kV/mm

Show Supplier Material materials with Dielectric strength of 27 kV/mm

IEC 60243-1

Volume resistivity

23.0 °C

1000000 Ω·cm

Show Supplier Material materials with Volume resistivity of 1000000 Ω·cm

IEC 60093

Rheological Properties

PropertyValueComment

Melt volume-flow rate

4 cm³/10min

Show Supplier Material materials with Melt volume-flow rate of 4 cm³/10min

ISO 1133, 230°C/10kg

Technological properties

Property
Application areas

Fuel Management - In-Tank and Fuel Venting Lines,Chemical Process Industry,Chemical Process Industry - Stock Shapes,Permanent Antistatic Solutions

Fillers