Kynar® 400 HDC M800

Alternative and trade names
PVDF-I
Want to keep this datasheet? Save it now in your required format

Description

Kynar® resins are fluorinated thermoplastic homopolymers.

Kynar® 400 HDC M800 resin is a thermoplastic fluorinated polymer. This product has been designed for Oil , Gas applications.

This material data has been provided by Arkema Technical Polymers.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyValueConditionTesting Standard

Density

1.73 g/cm³

Show Supplier Material materials with Density of 1.73 g/cm³

dry

ISO 1183

Mechanical

PropertyTemperatureValueConditionTesting StandardComment

Elastic modulus

1 GPa

Show Supplier Material materials with Elastic modulus of 1 GPa

dry

ISO 527-1/-2

Elongation

40 %

Show Supplier Material materials with Elongation of 40 %

dry

ISO 527-1/-2

min. | nominal

Elongation at yield

15 %

Show Supplier Material materials with Elongation at yield of 15 %

dry

ISO 527-1/-2

Impact strength, Charpy notched

-30 °C

10.6 kJ/m²

Show Supplier Material materials with Impact strength, Charpy notched of 10.6 kJ/m²

dry

ISO 179/1eA

23 °C

51 kJ/m²

Show Supplier Material materials with Impact strength, Charpy notched of 51 kJ/m²

dry

ISO 179/1eA

Impact strength, Charpy unnotched

No Break at 23 and -30°C

dry

ISO 179/1eU

Thermal

PropertyValueConditionTesting StandardPressureComment

Coefficient of thermal expansion

0.000183 1/K

Show Supplier Material materials with Coefficient of thermal expansion of 0.000183 1/K

dry

ISO 11359-1/-2

Heat deflection temperature

67 °C

Show Supplier Material materials with Heat deflection temperature of 67 °C

dry

ISO 75-1/-2

2 MPa

Melting point

171 °C

Show Supplier Material materials with Melting point of 171 °C

dry

ISO 11357-1/-3

10°C/min

Rheological Properties

PropertyValueConditionTesting StandardComment

Melt volume-flow rate

3 cm³/10min

Show Supplier Material materials with Melt volume-flow rate of 3 cm³/10min

dry

ISO 1133

230°C/10kg

Specific heat capacity melt

1600 J/(kg·K)

Show Supplier Material materials with Specific heat capacity melt of 1600 J/(kg·K)

Thermal conductivity of melt

0.19 W/(m·K)

Show Supplier Material materials with Thermal conductivity of melt of 0.19 W/(m·K)

Technological properties

Property
Application areas

Offshore Flexible Pipes

Processing methods

Injection Molding:

  • Melt temperature (°C) ISO 294: 230
  • Mold temperature (°C) ISO 10724: -
  • Injection velocity (mm/s) ISO 294: -
  • Pressure at hold (MPa) ISO 294: -