Kynar® resins are fluorinated thermoplastic homopolymers. This product is used for the co-extrusion of Rilsan® polyamides and Kynar® PVDF resins for the preparation of multilayer tubing or film.

This material data has been provided by Arkema Technical Polymers.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyValueConditionTesting Standard

Density

1.27 g/cm³

Show Supplier Material materials with Density of 1.27 g/cm³

dry

ISO 1183

Mechanical

PropertyValueTesting StandardConditionComment

Elongation

100 %

Show Supplier Material materials with Elongation of 100 %

ASTM D638

min.

Yield strength

35 MPa

Show Supplier Material materials with Yield strength of 35 MPa

ISO 527-1/-2

dry

Thermal

PropertyValueTesting Standard

Melting point

166 °C

Show Supplier Material materials with Melting point of 166 °C

ASTM D3418

Rheological Properties

PropertyValueTesting StandardConditionComment

Melt viscosity

160 Pa·s

Show Supplier Material materials with Melt viscosity of 160 Pa·s

ASTM D3835

Melt volume-flow rate

12.5 cm³/10min

Show Supplier Material materials with Melt volume-flow rate of 12.5 cm³/10min

ISO 1133

dry

230°C/10kg

Technological properties

Property
Application areas

Fuel Management - Fuel Lines