Kynar® ADX 111

Alternative and trade names
PVDF
Want to keep this datasheet? Save it now in your required format

Description

Outstanding characteristics: chemical resistance, imperviousness to UV, high barrier properties, high purity, good mechanical and thermo-mechanical properties.

Kynar® ADX 111 resin allows primer less powder coating (direct adhesion to metals after standard surface preparation.

Can be used easily in standard application processes:

  • Dip coating in fluidized bed
  • Electrostatic spraying
  • Hot flocking

  • This material data has been provided by Arkema High Performance Polymers.

    All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
    Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

    Ashby charts

    See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

    Properties

    General

    PropertyTemperatureValueComment

    Density

    23.0 °C

    1.78 g/cm³

    Show Supplier Material materials with Density of 1.78 g/cm³

    ISO 1183

    Limiting oxygen index

    23.0 °C

    44 %

    Show Supplier Material materials with Limiting oxygen index of 44 %

    ISO 4589-1/-2

    Moisture absorption

    23.0 °C

    0.07 %

    Show Supplier Material materials with Moisture absorption of 0.07 %

    Sim. to ISO 62

    Water absorption

    23.0 °C

    0.1 %

    Show Supplier Material materials with Water absorption of 0.1 %

    Sim. to ISO 62

    Mechanical

    PropertyTemperatureValueComment

    Elastic modulus

    23.0 °C

    2.2 GPa

    Show Supplier Material materials with Elastic modulus of 2.2 GPa

    ISO 527-1/-2

    Elongation

    23.0 °C

    50 %

    Show Supplier Material materials with Elongation of 50 %

    min., ISO 527-1/-2, nominal

    Elongation at yield

    23.0 °C

    8 %

    Show Supplier Material materials with Elongation at yield of 8 %

    ISO 527-1/-2

    Yield strength

    23.0 °C

    54 MPa

    Show Supplier Material materials with Yield strength of 54 MPa

    ISO 527-1/-2

    Thermal

    PropertyTemperatureValueComment

    Coefficient of thermal expansion

    23.0 °C

    1.5E-4 1/K

    Show Supplier Material materials with Coefficient of thermal expansion of 1.5E-4 1/K

    ISO 11359-1/-2

    Glass transition temperature

    -40 °C

    Show Supplier Material materials with Glass transition temperature of -40 °C

    ISO 11357-1/-2, 10°C/min

    Heat deflection temperature, 0.45 MPa

    132 °C

    Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 132 °C

    ISO 75-1/-2

    Heat deflection temperature, 1.80 MPa

    110 °C

    Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 110 °C

    ISO 75-1/-2

    Melting point

    169 °C

    Show Supplier Material materials with Melting point of 169 °C

    ISO 11357-1/-3, 10°C/min

    Vicat softening temperature

    139 °C

    Show Supplier Material materials with Vicat softening temperature of 139 °C

    ISO 306, 50°C/h 50N

    Flammability

    At thickness 1.5 mm IEC 60695-11-10: V-0, At thickness 0.8 mm IEC 60695-11-10: V-0

    Electrical

    PropertyTemperatureValueComment

    Comparative tracking index

    23.0 °C

    600 V

    Show Supplier Material materials with Comparative tracking index of 600 V

    IEC 60112

    Dielectric constant, 100Hz

    23.0 °C

    9 [-]

    Show Supplier Material materials with Dielectric constant, 100Hz of 9 [-]

    IEC 60250

    Dielectric constant, 1MHz

    23.0 °C

    7 [-]

    Show Supplier Material materials with Dielectric constant, 1MHz of 7 [-]

    IEC 60250

    Dielectric strength

    23.0 °C

    21 kV/mm

    Show Supplier Material materials with Dielectric strength of 21 kV/mm

    IEC 60243-1

    Dissipation factor, 100Hz

    23.0 °C

    0.03 [-]

    Show Supplier Material materials with Dissipation factor, 100Hz of 0.03 [-]

    IEC 60250

    Dissipation factor, 1MHz

    23.0 °C

    0.21 [-]

    Show Supplier Material materials with Dissipation factor, 1MHz of 0.21 [-]

    IEC 60250

    Volume resistivity

    23.0 °C

    2.00E+14 Ω·cm

    Show Supplier Material materials with Volume resistivity of 2.00E+14 Ω·cm

    IEC 60093

    Rheological Properties

    PropertyValueComment

    Melt volume-flow rate

    27 cm³/10min

    Show Supplier Material materials with Melt volume-flow rate of 27 cm³/10min

    ISO 1133, 230°C/3.8kg

    Technological properties

    Property
    Application areas

    Main applications:

  • corrosion protection in the chemical industry
  • coating (painting, co-extrusion)
  • off-shore
  • wire and cable
  • PPA
  • attery

    or

    Metal Tube Coating