Kynar® resins are fluorinated thermoplastic homopolymers.

Kynar® ADX 1285-03 resin is a flexible thermoplastic fluorinated functionalized polymer. The properties are the same as standard grade: chemical resistance, resistance to UV, low permeation, high purity, excellent mechanical behavior. More over, these grades increase the potential of adhesion on materials as polyamides, polyolefins and can be coextruded.

This material data has been provided by Arkema Technical Polymers.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyValueConditionTesting Standard

Density

1.78 g/cm³

Show Supplier Material materials with Density of 1.78 g/cm³

dry

ISO 1183

Mechanical

PropertyValueConditionTesting StandardComment

Elongation

50 %

Show Supplier Material materials with Elongation of 50 %

dry

ISO 527-1/-2

min. | nominal

Elongation at yield

10 %

Show Supplier Material materials with Elongation at yield of 10 %

dry

ISO 527-1/-2

Yield strength

42 MPa

Show Supplier Material materials with Yield strength of 42 MPa

dry

ISO 527-1/-2

Thermal

PropertyValueConditionTesting StandardPressureComment

Heat deflection temperature

72 °C

Show Supplier Material materials with Heat deflection temperature of 72 °C

dry

ISO 75-1/-2

2 MPa

Melting point

165 °C

Show Supplier Material materials with Melting point of 165 °C

dry

ISO 11357-1/-3

10°C/min

Flammability

At thickness 0.8 mm IEC 60695-11-10: HB

Technological properties

Property
Application areas

Chemical Process Industry,Underground Fuel Containment