Kynar® Film 502 CUH HC

Alternative and trade names
PVDF
Want to keep this datasheet? Save it now in your required format

Description

Kynar® Film 502 CUH HC is flexible thermoplastic fluorinated film. The properties are the same as standard grade: chemical resistance, resistance to UV, low permeation, high purity, excellent mechanical behavior. These films are specially designed for architectural applications.

This material data has been provided by Arkema Technical Polymers.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyValueConditionTesting Standard

Density

1.36 g/cm³

Show Supplier Material materials with Density of 1.36 g/cm³

dry

ISO 1183

Mechanical

PropertyValueConditionTesting StandardComment

Elongation

50 %

Show Supplier Material materials with Elongation of 50 %

dry

ISO 527-3

Transverse

50 %

Show Supplier Material materials with Elongation of 50 %

dry

ISO 527-3

Elongation at yield

3.5 %

Show Supplier Material materials with Elongation at yield of 3.5 %

dry

ISO 527-3

Elongation at yield, transverse

3.5 %

Show Supplier Material materials with Elongation at yield, transverse of 3.5 %

dry

ISO 527-3

Tear strength

2 kN/m

Show Supplier Material materials with Tear strength of 2 kN/m

ISO 6383-1

3 kN/m

Show Supplier Material materials with Tear strength of 3 kN/m

ISO 6383-1

Transverse

Tensile strength

25 MPa

Show Supplier Material materials with Tensile strength of 25 MPa

dry

ISO 527-3

Transverse

30 MPa

Show Supplier Material materials with Tensile strength of 30 MPa

dry

ISO 527-3

Electrical

PropertyValueConditionTesting Standard

Dielectric strength

100 kV/mm

Show Supplier Material materials with Dielectric strength of 100 kV/mm

dry

IEC 60243-1

Technological properties

Property
Application areas

Photovoltaic / Solar Film