Description

Kynar® HSV1810 is a functional homopolymer of vinylidene fluoride, specifically designed to be used as a cathode binder in Lithium Ion Batteries. Main Characteristics:

  • High adhesion
  • Excellent cathode slurry stability with Nickel Rich Active Materials
  • High molecular weight
  • Functional

  • This material data has been provided by Arkema Technical Polymers.

    All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
    Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

    Ashby charts

    Properties

    General

    PropertyValueTesting StandardComment

    Density

    1.78 g/cm³

    Show Supplier Material materials with Density of 1.78 g/cm³

    ASTM D792

    min.

    Thermal

    PropertyValueTesting Standard

    Melting point

    161 - 167 °C

    Show Supplier Material materials with Melting point of 161 - 167 °C

    ASTM D3418

    Rheological Properties

    PropertyValueTesting Standard

    Melt viscosity

    7000 - 7500 Pa·s

    Show Supplier Material materials with Melt viscosity of 7000 - 7500 Pa·s

    ASTM D3835

    Technological properties

    Property
    Application areas

    Lithium Ion Battery Binder