Orgalloy® EM 067 HSP

Alternative and trade names
PA6
Want to keep this datasheet? Save it now in your required format

Description

Orgalloy® EM 067 HSP resin is a flexible polyamide designed to be used for refrigerant barrier layer in air conditioning rubber hose.

Packaging:

This grade is delivered dried in sealed packaging (20kg bags) ready to be processed.

Shelf life:

Two years from the date of delivery. For any use above this limit, please refer to our technical services.

This material data has been provided by Arkema Technical Polymers.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyValueConditionTesting Standard

Density

1.14 g/cm³

Show Supplier Material materials with Density of 1.14 g/cm³

dry

ISO 1183

Mechanical

PropertyValueConditionTesting StandardComment

Elastic modulus

0.572 GPa

Show Supplier Material materials with Elastic modulus of 0.572 GPa

cond.

ISO 527-1/-2

Elongation

50 %

Show Supplier Material materials with Elongation of 50 %

cond.

ISO 527-1/-2

min.

Yield strength

28 MPa

Show Supplier Material materials with Yield strength of 28 MPa

dry

ISO 527-1/-2

Thermal

PropertyValueConditionTesting StandardComment

Melting point

215 °C

Show Supplier Material materials with Melting point of 215 °C

dry

ISO 11357-1/-3

10°C/min

Rheological Properties

PropertyValueConditionTesting StandardComment

Melt volume-flow rate

1 cm³/10min

Show Supplier Material materials with Melt volume-flow rate of 1 cm³/10min

dry

ISO 1133

235°C/5kg

Technological properties

Property
Application areas

Fluid Management - Air Conditioning Circuit

Processing methods

Extrusion:

  • Drying time (only necessary for bags opened for more than two hours): 4-16 hours at 80-90°C
  • Extrusion melt temperature (min-recommended-max): 240-260-300°C