Orgasol® 1002 ES5 NAT 1

Alternative and trade names
PA6
Want to keep this datasheet? Save it now in your required format

Description

ORGASOL® 1002 ES5 NAT 1 is spheroidal polyamide 6 powder with a narrow particle size distribution and an average diameter of 50µm.

Orgasol® 1002 ES5 NAT 1 has a high melting temperature, above 210°C: the shape of the particles and the particle size distribution are preserved even when processed at high temperatures. An extremely high level of quality is achieved through rigorous control of the particle size distribution , porosity, ensuring excellent consistency of performance.

ORGASOL® is a range of high performance ultra-fine polyamide powders used as multifunctional additives in coatings, inks, varnishes and technical compounds.

The introduction of ORGASOL® polyamide powders in formulations is easy thanks to their good dispersion capacity, their reduced Impact on rheology and their low density.

ORGASOL® polyamide powders are surface modifiers, specifically designed for gloss control, texture creation and haptic properties adjustment. They also improve blocking resistance and reduce coefficient of friction.

Abrasion, scratch, impact resistances and flexibility of coatings, inks and varnishes and technical compounds can be significantly improved using ORGASOL® polyamide powders.

This material data has been provided by Arkema High Performance Polymers.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyTemperatureValueComment

Coarse particles amount

5 %

Show Supplier Material materials with Coarse particles amount of 5 %

max., ISO 13319

Coarse particles size

70 μm

Show Supplier Material materials with Coarse particles size of 70 μm

min.

Density

23.0 °C

0.43 g/cm³

Show Supplier Material materials with Density of 0.43 g/cm³

ISO 1068, apparent density unpacked

Fine particles amount

5 %

Show Supplier Material materials with Fine particles amount of 5 %

max., ISO 13319

Fine particles size

30 μm

Show Supplier Material materials with Fine particles size of 30 μm

max.

Median particles size

50 μm

Show Supplier Material materials with Median particles size of 50 μm

ISO 13319

Specific surface area

1 m²/g

Show Supplier Material materials with Specific surface area of 1 m²/g

ISO 9277

Thermal

PropertyValueComment

Melting point

217 °C

Show Supplier Material materials with Melting point of 217 °C

ISO 11357-3

Technological properties

Property
Application areas

Main applications:

  • Coil coating
  • Floor coating
  • Wood coating
  • Plastic coating

    or

    Coating Additives - Coil Coating,Coating Additives - Rubber Coating

  • Other

    Packaging This grade is delivered in 20kg bag.

    Shelf Life Three years from the date of delivery. For any use after this limit, please refer to our technical services.