Orgasol® 2002 EXD NAT 1

Alternative and trade names
PA12
Want to keep this datasheet? Save it now in your required format

Description

ORGASOL® 2002 EXD NAT 1 is spheroidal polyamide 12 powder with a narrow particle size distribution and an average diameter of 10µm. ORGASOL® 2002 EXD NAT 1 has a melting temperature of 177°C. An extremely high level of quality is achieved through rigorous control of the particle size distribution , porosity, ensuring excellent consistency of performance.

ORGASOL® is a range of high performance ultra-fine polyamide powders used as multifunctional additives in coatings, inks, varnishes and technical compounds.

The introduction of ORGASOL® polyamide powders in formulations is easy thanks to their good dispersion capacity, their reduced Impact on rheology and their low density.

ORGASOL® polyamide powders are surface modifiers, specifically designed for gloss control, texture creation and haptic properties adjustment. They also improve blocking resistance and reduce coefficient of friction.

Abrasion, scratch, impact resistances and flexibility of coatings, inks and varnishes and technical compounds can be significantly improved using ORGASOL® polyamide powders.

This material data has been provided by Arkema Technical Polymers.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyValueTesting StandardComment

Coarse particles amount

2 %

Show Supplier Material materials with Coarse particles amount of 2 %

ISO 13319

max.

Coarse particles size

20 μm

Show Supplier Material materials with Coarse particles size of 20 μm

min.

Density

0.375 g/cm³

Show Supplier Material materials with Density of 0.375 g/cm³

ISO 1068

apparent density unpacked

Fine particles amount

2 %

Show Supplier Material materials with Fine particles amount of 2 %

ISO 13319

max.

Fine particles size

5 μm

Show Supplier Material materials with Fine particles size of 5 μm

max.

Median particles size

10 μm

Show Supplier Material materials with Median particles size of 10 μm

ISO 13319

Specific surface area

1.5 m²/g

Show Supplier Material materials with Specific surface area of 1.5 m²/g

ISO 9277

Thermal

PropertyValueConditionTesting Standard

Melting point

177 °C

Show Supplier Material materials with Melting point of 177 °C

dry

ISO 11357-3

Technological properties

Property
Application areas

Coating Additives - Can Coating,Coating Additives - Inks-OPVs