Description

ORGASOL® 3502 D NAT 1 is spheroidal copolyamide 6/12 powder with a narrow particle size distribution and an average diameter of 20µm. ORGASOL® 3502 D NAT 1 has a melting temperature of 142°C. An extremely high level of quality is achieved through rigorous control of the particle size distribution , porosity, ensuring excellent consistency of performance.

ORGASOL® is a range of high performance ultra-fine polyamide powders used as multifunctional additives in coatings, inks, varnishes and technical compounds.

The introduction of ORGASOL® polyamide powders in formulations is easy thanks to their good dispersion capacity, their reduced Impact on rheology and their low density.

ORGASOL® polyamide powders are surface modifiers, specifically designed for gloss control, texture creation and haptic properties adjustment. They also improve blocking resistance and reduce coefficient of friction.

Abrasion, scratch, impact resistances and flexibility of coatings, inks and varnishes and technical compounds can be significantly improved using ORGASOL® polyamide powders.

This material data has been provided by Arkema High Performance Polymers.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyTemperatureValueComment

Coarse particles amount

5 %

Show Supplier Material materials with Coarse particles amount of 5 %

max., ISO 13319

Coarse particles size

30 μm

Show Supplier Material materials with Coarse particles size of 30 μm

min.

Density

23.0 °C

0.38 g/cm³

Show Supplier Material materials with Density of 0.38 g/cm³

ISO 1068, apparent density unpacked

Fine particles amount

5 %

Show Supplier Material materials with Fine particles amount of 5 %

max., ISO 13319

Fine particles size

10 μm

Show Supplier Material materials with Fine particles size of 10 μm

max.

Median particles size

20 μm

Show Supplier Material materials with Median particles size of 20 μm

ISO 13319

Specific surface area

6 m²/g

Show Supplier Material materials with Specific surface area of 6 m²/g

ISO 9277

Thermal

PropertyValueComment

Melting point

142 °C

Show Supplier Material materials with Melting point of 142 °C

ISO 11357-3

Technological properties

Property
Application areas

Main applications:

  • Metal Injection Molding Powder Injection Molding
  • Ceramic Injection Molding
  • Wood coating
  • Plastic coating
  • Transfer paper for inkjet

    or

    Coating Additives - Inkjet Transfer Paper,Coating Additives - Metal Injection Molding

  • Other

    Packaging This grade is delivered in 15kg bag.

    Shelf Life Three years from the date of delivery. For any use after this limit, please refer to our technical services.