Pebax® 2533 SA 01 MED

Alternative and trade names
TPA
Want to keep this datasheet? Save it now in your required format

Description

Polyether block amide Pebax® 2533 SA 01 MED resin is a thermoplastic elastomer made of flexible polyether and rigid polyamide. This grade offers the highest quality and it is specially designed to meet the stringent requirements of the medical applications such as minimally invasive devices. Upon request, letters regarding USP Class VI compliance can be provided.

This material data has been provided by Arkema Technical Polymers.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyValueConditionTesting Standard

Density

1 g/cm³

Show Supplier Material materials with Density of 1 g/cm³

dry

ISO 1183

Moisture absorption

0.4 %

Show Supplier Material materials with Moisture absorption of 0.4 %

Sim. to ISO 62

Water absorption

1.2 %

Show Supplier Material materials with Water absorption of 1.2 %

Sim. to ISO 62

Mechanical

PropertyValueConditionTesting StandardComment

Elastic modulus

0.01 GPa

Show Supplier Material materials with Elastic modulus of 0.01 GPa

cond.

ISO 527-1/-2

0.012 GPa

Show Supplier Material materials with Elastic modulus of 0.012 GPa

dry

ISO 527-1/-2

Elongation

50 %

Show Supplier Material materials with Elongation of 50 %

cond., dry

ISO 527-1/-2

min.

Hardness, Shore A

77 [-]

Show Supplier Material materials with Hardness, Shore A of 77 [-]

ISO 7619-1

for 3 seconds

Hardness, Shore D

22 [-]

Show Supplier Material materials with Hardness, Shore D of 22 [-]

dry

ISO 7619-1

15 seconds

Impact strength, Charpy notched

No Break at 23 and -30°C

dry and cond.

ISO 179/1eA

Impact strength, Charpy unnotched

No Break at 23 and -30°C

dry and cond.

ISO 179/1eU

Thermal

PropertyValueConditionTesting StandardComment

Melting point

134 °C

Show Supplier Material materials with Melting point of 134 °C

dry

ISO 11357-1/-3

10°C/min

Vicat softening temperature

58 °C

Show Supplier Material materials with Vicat softening temperature of 58 °C

ISO 306

50°C/h 50N

Rheological Properties

PropertyValueConditionTesting StandardComment

Shrinkage

0.5 %

Show Supplier Material materials with Shrinkage of 0.5 %

dry

ISO 294-4

0.8 %

Show Supplier Material materials with Shrinkage of 0.8 %

dry

ISO 294-4

Transverse

Technological properties

Property
Application areas

Healthcare-Other,IV Bags,Medical Catheters

Certifications

USP Class VI

Processing methods

Injection Molding:

  • Typical melt temperature (Min / Recommended / Max) : 180°C / 210°C / 240°C.
  • Typical mold temperature : 10 – 30°C.
  • Drying time and temperature (only necessary for bags opened for more than two hours) : 4-8 hours at 55-65°C.