Description

Polyether block amide Pebax® 5533 SP 01 resin is a thermoplastic elastomer made of flexible polyether and rigid polyamide. This SP grade has been developed to be heat and UV resistant.

This material data has been provided by Arkema High Performance Polymers.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValueComment

Abrasion resistance

47 mm³

Show Supplier Material materials with Abrasion resistance of 47 mm³

ISO 4649

Density

23.0 °C

1.01 g/cm³

Show Supplier Material materials with Density of 1.01 g/cm³

ISO 1183

Moisture absorption

23.0 °C

0.6 %

Show Supplier Material materials with Moisture absorption of 0.6 %

Sim. to ISO 62

Water absorption

23.0 °C

1.2 %

Show Supplier Material materials with Water absorption of 1.2 %

Sim. to ISO 62

Mechanical

PropertyTemperatureValueComment

Compression set

23.0 °C

43 [-]

Show Supplier Material materials with Compression set of 43 [-]

ISO 815, 24h

Elastic modulus

23.0 °C

0.17 GPa

Show Supplier Material materials with Elastic modulus of 0.17 GPa

ISO 527-1/-2

Elongation

23.0 °C

50 %

Show Supplier Material materials with Elongation of 50 %

min., ISO 527-1/-2, nominal

Elongation at yield

23.0 °C

25 %

Show Supplier Material materials with Elongation at yield of 25 %

ISO 527-1/-2

Hardness, Shore D

23.0 °C

50 [-]

Show Supplier Material materials with Hardness, Shore D of 50 [-]

ISO 7619-1, 15 seconds

Tear strength

23.0 °C

106 kN/m

Show Supplier Material materials with Tear strength of 106 kN/m

ISO 34-1

Yield strength

23.0 °C

12 MPa

Show Supplier Material materials with Yield strength of 12 MPa

ISO 527-1/-2

Impact strength, Charpy notched

No break @ 23,-30°C, ISO 179/1eA

Impact strength, Charpy unnotched

No break @ 23,-30°C, ISO 179/1eU

Thermal

PropertyTemperatureValueComment

Coefficient of thermal expansion

23.0 °C

1.7E-4 1/K

Show Supplier Material materials with Coefficient of thermal expansion of 1.7E-4 1/K

ISO 11359-1/-2

Heat deflection temperature, 0.45 MPa

66 °C

Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 66 °C

ISO 75-1/-2

Melting point

159 °C

Show Supplier Material materials with Melting point of 159 °C

ISO 11357-1/-3, 10°C/min

Vicat softening temperature

142 °C

Show Supplier Material materials with Vicat softening temperature of 142 °C

ISO 306, 50°C/h 50N

Flammability

At thickness 1.6 mm IEC 60695-11-10: HB and yellow card available

Electrical

PropertyTemperatureValueComment

Comparative tracking index

23.0 °C

600 V

Show Supplier Material materials with Comparative tracking index of 600 V

IEC 60112, Conditioned

Dielectric constant, 100Hz

23.0 °C

9 [-]

Show Supplier Material materials with Dielectric constant, 100Hz of 9 [-]

IEC 60250

Dielectric constant, 1MHz

23.0 °C

5 [-]

Show Supplier Material materials with Dielectric constant, 1MHz of 5 [-]

IEC 60250

Dielectric strength

23.0 °C

38.5 kV/mm

Show Supplier Material materials with Dielectric strength of 38.5 kV/mm

IEC 60243-1

Dissipation factor, 100Hz

23.0 °C

0.11 [-]

Show Supplier Material materials with Dissipation factor, 100Hz of 0.11 [-]

IEC 60250

Dissipation factor, 1MHz

23.0 °C

0.1 [-]

Show Supplier Material materials with Dissipation factor, 1MHz of 0.1 [-]

IEC 60250

Volume resistivity

23.0 °C

3.20E+13 Ω·cm

Show Supplier Material materials with Volume resistivity of 3.20E+13 Ω·cm

IEC 60093

Rheological Properties

PropertyTemperatureValueComment

Density of melt

0.83 g/cm³

Show Supplier Material materials with Density of melt of 0.83 g/cm³

Shrinkage

23.0 °C

1.2 %

Show Supplier Material materials with Shrinkage of 1.2 %

ISO 294-4 2577

Shrinkage, transverse

23.0 °C

1.4 %

Show Supplier Material materials with Shrinkage, transverse of 1.4 %

ISO 294-4 2577

Specific heat capacity melt

2800 J/(kg·K)

Show Supplier Material materials with Specific heat capacity melt of 2800 J/(kg·K)

Thermal conductivity of melt

0.18 W/(m·K)

Show Supplier Material materials with Thermal conductivity of melt of 0.18 W/(m·K)

Technological properties

Property
Application areas

Main applications:

  • Athletic foot wear components
  • Ski shoes
  • High performance power trasmission belts

    or

    Conveyor Belts and Pulleys,Packaging / Film,Permanent Antistatic Solutions,Pneumatic Tubing,Hook and Loop Fasteners,Textile - Others,Footwear - Midsoles / Foam,Footwear - Outsoles,Ski Boots

  • Other

    Packaging:

  • This grade is delivered dried in sealed packaging (20 or 25 kg bags) ready to be processed.

    Shelf life:

  • Two years from the delivery. For any use above this limit, please refer to our technical services.

  • Processing methods

    Injection Molding:

  • Typical melt temperature (Min / Recommended / Max) : 200°C / 240°C / 270°C.
  • Typical mold temperature : 25 – 60°C.
  • Drying time and temperature (only necessary for bags opened for more than two hours) : 4-6 hours at 65-75°C.


    Extrusion:

  • Typical melt temperature (Min / Recommended / Max) : 210°C / 220°C / 230°C
  • Drying time and temperature (only necessary for bags opened for more than two hours) : 4-6 hours at 65-75°C